- What melts in
- Hollow wire with flux inside, fed from a spool
- Shielding
- Flux in the wire (self-shielded types need no gas)
- Current
- Usually DC, electrode negative for self-shielded wire
- Slag
- Thin layer to chip off
- In wind
- Good: the flux makes its own shield
How flux-core works
As the arc melts the tubular wire, the flux inside burns and melts too. Part of it turns into gas that pushes air away from the puddle. The rest floats to the top and hardens into a layer of slag that protects the cooling weld. The formal name is flux-cored arc welding, or FCAW.
There are two kinds of flux-core wire:
- Self-shielded wire makes all its own protection. This is the kind small hobby machines run, and it is the reason flux-core is popular for outdoor work.
- Gas-shielded wire (often called dual shield) uses flux and bottled gas together. It is common in fabrication shops for thick steel, and it needs a still-air setting like MIG.
Polarity matters
Self-shielded flux-core wire usually runs on DC electrode negative, the opposite of MIG. On many machines you switch by moving two leads inside the cabinet. The wire package states the correct polarity. Running the wrong one gives a harsh arc, heavy spatter and poor fusion, and it is one of the most common beginner mistakes.
Flux-core wire is softer than solid wire, so most machines use knurled drive rolls for it. Too much roll tension crushes the wire. The machine manual explains the swap.
Technique
- Clean the metal where you can. Flux-core forgives some mill scale and light rust, but clean steel still welds better.
- Use a little more wire stickout than with MIG. The wire package often gives a range.
- Drag the gun, pointing back at the finished weld, at about 10 to 20 degrees. A common saying is "if there's slag, you drag."
- Keep the slag behind the puddle. If it runs ahead, it can get trapped in the weld.
- Let the weld cool a little, then chip the slag off with a chipping hammer and brush the bead before the next pass.
Chipped slag flies off hot and sharp. Keep safety glasses on under your helmet and when you lift the helmet to chip.
Strengths and trade-offs
Flux-core keeps working in a breeze, penetrates well into thicker steel, and frees you from a gas cylinder. That makes it a good fit for fence posts, trailers, gates and farm repairs. The trade-offs are more spatter, more smoke, slag to clean off every pass, and a rougher-looking bead than MIG. Self-shielded wire is mainly a steel process. Fumes are heavy, so ventilation matters even outdoors: keep your head out of the plume. See ventilation and fire safety.
Common problems
| What you see | Likely cause |
|---|---|
| Slag lines trapped in the weld | Pushing instead of dragging, or not cleaning between passes |
| Wormholes or porosity | Wrong polarity, too short a stickout, or damp wire |
| Heavy spatter | Wrong polarity, or voltage set too high |
| Wire crushed or bird-nesting at the rolls | Too much drive roll tension or the wrong rolls |
Compare it with the other processes on choosing a process, or read the MIG explainer for the gas-shielded side of the same machine.
Flux-core questions
Can I run flux-core wire in a MIG machine?
Many small MIG machines can, if they have switchable polarity and the right drive rolls. The manual says whether yours can and how to set it up.
Can flux-core weld aluminum?
Common flux-core wire is made for steel. Aluminum is usually welded with MIG using pure argon or with TIG.