Weld Blog

Process ยท GMAW

MIG welding explained

MIG welding feeds a solid wire through a gun while shielding gas flows around it. Pull the trigger and the wire, the current and the gas all start together, which makes it the usual first process for beginners.

What melts in
Solid wire fed from a spool by the gun
Shielding
Bottled shielding gas
Current
DC, electrode positive
Slag
None
In wind
Poor: a breeze blows the gas away

How MIG works

The machine pushes a spool of thin solid wire through a liner to the gun. When you press the trigger, current flows through the wire, an arc forms where the wire meets the work, and the wire melts into the joint as filler. At the same time, shielding gas flows out of the nozzle and pushes air away from the molten puddle. The formal name is gas metal arc welding, or GMAW.

The ground clamp (properly called the work clamp) completes the circuit, so it needs to sit on clean, bare metal close to the weld.

The two main settings

Most MIG machines give you two controls that work together:

  • Voltage sets the arc length and how wide and flat the bead spreads.
  • Wire feed speed sets how much wire goes in, and with it the current. More wire means more heat and more filler.

Machines come with a chart, usually inside the door that covers the spool, that gives starting settings for each wire size and metal thickness. Start there, run a test bead on scrap of the same thickness, and adjust. A well-tuned short-circuit MIG arc makes a steady crackle that many welders compare to bacon frying.

Shielding gas

For mild steel, a mix of about 75 percent argon and 25 percent carbon dioxide is the common choice for small machines. It gives a smooth arc and little spatter. Straight carbon dioxide also works on steel and digs in deeper, with more spatter. Aluminum needs pure argon. The gas cylinder should be chained upright, with the regulator set to the flow the manual suggests.

Gun angle and travel

  1. Clean the metal to bright steel with a grinder or wire brush where the weld and ground clamp go.
  2. Trim the wire so about 1/4 to 3/8 inch sticks out past the contact tip.
  3. Hold the gun at a slight angle, about 10 to 15 degrees from straight up, in the direction of travel.
  4. Push the gun (pointing ahead of the puddle) for a flatter bead, or drag it for a little more penetration. Many welders push MIG on steel.
  5. Watch the leading edge of the puddle and move at a pace that keeps the bead an even width.

Common problems

What you seeLikely cause
Holes and bubbles in the bead (porosity)Not enough gas, an empty cylinder, a draft, or dirty metal
Tall, narrow bead sitting on topToo cold, or moving too fast
Holes burned through thin metalToo hot, or moving too slowly
Lots of spatterSettings out of balance, too much wire stickout, or wrong polarity
Wire jams or stuttersWorn contact tip, wrong drive roll tension, or a kinked liner

Where MIG falls short

Wind is the big one. A breeze or a strong shop fan strips the gas away and leaves porous welds, which is why outdoor repairs often switch to flux-core or stick. MIG also needs clean metal, and the gas cylinder adds weight if you need to move the setup around.

Before your first bead, read safety gear and ventilation and fire safety, then work through the practice ladder.

MIG questions

What does MIG stand for?

Metal inert gas. The name stuck even though the common steel mix includes carbon dioxide, which is not inert. The formal term is gas metal arc welding (GMAW).

What wire size should a beginner use?

Small machines usually run wire about 0.023 to 0.035 inch thick. The machine's chart lists which sizes it handles and what thickness of metal each one suits.